Description
Features and Applications
Suitabilty for use in out-of-position welding except for welding at vertical down position.
Excellent strength and toughness.
Suitability for the formation of welding buffer layers when building up high-carbon steels.
Weld deposits with very low hydrogen content.
Weld metal recovery of about 120%.
Requirement of re-drying for minimum 2 hours at the temperatures between 300°C and 350°C.